Schematic of rippled-interface sample preparation (a) A surface structure
of photoresist and anti-reflective coating (ARC) capped with tungsten is
produced using x-ray lithography. The exposed surface is reactive-ion
etched.
(b) Ion-implantation through the resulting periodic surface structure
results in a rippled a-c interface.